Continuous Casting Center

Modeling of Continuous-Casting Defects Related to Mold Fluid Flow

Thomas, B. G

3rd Internat. Congress on Science & Technology of Steelmaking, Charlotte, NC, May 9-11, 2005, Association for Iron & Steel Technology, Warrendale, PA, 847-861, 2005. [keynote paper]

2005

Cite this publication

Thomas, B. G, "Modeling of Continuous-Casting Defects Related to Mold Fluid Flow", 3rd Internat. Congress on Science & Technology of Steelmaking, Charlotte, NC, May 9-11, 2005, Association for Iron & Steel Technology, Warrendale, PA, 847-861, 2005. [keynote paper] (2005).

Trouble viewing the PDF here?Open it in a new tab.